추천 제품
vapor pressure
<0.01 mmHg ( 25 °C)
<1 mmHg ( 20 °C)
형태
solid
분자량
average Mn ~2,000
포함
BHT as stabilizer
mp
28-40 °C
density
0.972 g/mL at 25 °C
SMILES string
OCCCCO
InChI
1S/C8H18O2/c1-3-5-6-10-8(4-2)7-9/h8-9H,3-7H2,1-2H3/t8-/m0/s1
InChI key
BJZYYSAMLOBSDY-QMMMGPOBSA-N
유사한 제품을 찾으십니까? 방문 제품 비교 안내
애플리케이션
Poly(tetrahydrofuran) (PTHF) can be used as a macroinitiator to prepare block copolymers via ring-opening polymerization.
Cross-linked PTHF can be used as a matrix to prepare thermally stable polymer electrolytes for lithium-ion batteries.
It can also be used as a starting material to prepare cyclodextrin-basedsupramolecular complexes for drug and gene delivery.
Cross-linked PTHF can be used as a matrix to prepare thermally stable polymer electrolytes for lithium-ion batteries.
It can also be used as a starting material to prepare cyclodextrin-basedsupramolecular complexes for drug and gene delivery.
법적 정보
Product of DuPont
Terathane is a registered trademark of Invista North America S.a.r.l.
유해 및 위험 성명서
예방조치 성명서
Hazard Classifications
Aquatic Chronic 3
Storage Class Code
10 - Combustible liquids
WGK
WGK 3
개인 보호 장비
dust mask type N95 (US), Eyeshields, Gloves
시험 성적서(COA)
제품의 로트/배치 번호를 입력하여 시험 성적서(COA)을 검색하십시오. 로트 및 배치 번호는 제품 라벨에 있는 ‘로트’ 또는 ‘배치’라는 용어 뒤에서 찾을 수 있습니다.
Journal of biomedical materials research, 49(1), 99-105 (1999-11-24)
Interaction of macrophages (Mos) with polyetherurethane (PEU) was investigated to clarify the role of the Mos in the early stage of tumorigenesis of PEUs. As for the inflammatory cytokines produced from Mos, the amount of tumor necrosis factor (TNF) produced
Journal of colloid and interface science, 277(2), 304-308 (2004-09-03)
Aqueous dispersions of poly(ester-imide)s [P(E-I)s] have been prepared by dispersing the P(E-I)s in water without any external solubilizing agents. P(E-I)s were prepared from anhydride-terminated polyester prepolymer and diisocyanate. The -COOH groups in the polymer were then neutralized using triethylamine and
Journal of biomaterials science. Polymer edition, 5(3), 231-244 (1993-01-01)
Poly(etherurethane urea) (PEUU) elastomers when employed as biomedical devices may be susceptible to extraction upon implantation. Four PEUU elastomers containing a single PEUU formulation, but varying in terms of their additives, were subjected to an in vitro extraction procedure. The
Biomaterials, 23(8), 1797-1808 (2002-04-13)
In vitro protein adsorption, platelet adhesion and activation on new hydrogel surfaces, composed of poly(ethylene oxide) (PEO) and poly(tetramethylene oxide) (PTMO) or poly(dimethyl siloxane) (PDMS), were investigated. By varying PEO length (MW = 2000 or 3400), hydrophobic components (PTMO or
Journal of biomaterials science. Polymer edition, 13(5), 527-542 (2002-08-17)
A multiblock copolymer composed of poly(ethylene oxide) (PEO) and poly(tetramethylene oxide) (PTMO) and which forms a physical hydrogel was blended with Pellethane, a commercial segmented polyurethane (SPU) developed for various biomedical devices, to provide a PEO-rich surface with improved stability.
자사의 과학자팀은 생명 과학, 재료 과학, 화학 합성, 크로마토그래피, 분석 및 기타 많은 영역을 포함한 모든 과학 분야에 경험이 있습니다..
고객지원팀으로 연락바랍니다.