Poly(ethyl methacrylate)

average Mw ~515,000 by GPC, powder

동의어(들):

Ethyl methacrylate homopolymer, Poly(ethyl 2-methyl-2-propeonate)

로그인조직 및 계약 가격 보기


About This Item

Linear Formula:
[CH2C(CH3)(CO2C2H5)]n
CAS Number:
MDL number:
UNSPSC 코드:
41116107
PubChem Substance ID:
NACRES:
NA.23

양식

powder

분자량

average Mw ~515,000 by GPC

refractive index

n20/D 1.485

내재 점도

0.80 dL/g(lit.)

전이 온도

Tg 63 °C

density

1.11 g/mL at 25 °C

SMILES string

CCOC(=O)C(C)=C

InChI

1S/C6H10O2/c1-4-8-6(7)5(2)3/h2,4H2,1,3H3

InChI key

SUPCQIBBMFXVTL-UHFFFAOYSA-N

유사한 제품을 찾으십니까? 방문 제품 비교 안내

일반 설명

PEMA is known to exhibit biocompatibility and in vivo stability in its various use in implants and medical devices. Sorption of low solubility gases in PEMA was observed to be comparatively lower that polymers with high transition temperature.

애플리케이션

Poly(ethyl methacrylate) (PEMA) may be used to prepare polymer blends with polystyrene using organically modified clay as emulsifier.

Storage Class Code

10 - Combustible liquids

WGK

WGK 3

Flash Point (°F)

Not applicable

Flash Point (°C)

Not applicable


가장 최신 버전 중 하나를 선택하세요:

시험 성적서(COA)

Lot/Batch Number

적합한 버전을 찾을 수 없으신가요?

특정 버전이 필요한 경우 로트 번호나 배치 번호로 특정 인증서를 찾을 수 있습니다.

이 제품을 이미 가지고 계십니까?

문서 라이브러리에서 최근에 구매한 제품에 대한 문서를 찾아보세요.

문서 라이브러리 방문

Gas sorption and permeation in poly (ethyl methacrylate).
Chiou J S and Paul D R
Journal of Membrane Science , 45(1-2), 167-189 (1989)
Emulsifying effect of dimethyldioctadecylammonium-hectorite in polystyrene/poly (ethyl methacrylate) blends.
Voulgaris D and Petridis D
Polymer, 43(8), 2213-2218 (2002)
Assessment of the parameters influencing the fiber characteristics of electrospun poly (ethyl methacrylate) membranes.
Gomez-Tejedor J A, et al.
European Polymer Journal, 47(2), 119-129 (2011)
Ronald D Perry et al.
Compendium of continuing education in dentistry (Jamesburg, N.J. : 1995), 33(1), 59-60 (2012-03-22)
Clinicians have many choices of provisional materials from which to choose when fabricating interim fixed restorations. While traditional materials are still in use today, temporary materials are continuously being updated and improved upon. In addition to the functional necessities required
Yutaka Takahashi et al.
Gerodontology, 29(2), e1086-e1091 (2012-01-21)
This study investigated the fracture resistance of maxillary acrylic resin complete dentures subjected to long-term water immersion. Maxillary acrylic resin complete dentures were fabricated from five denture base resins. Half of the dentures were stored in water for 50 h

문서

Self-assembled monolayers (SAMs) have diverse applications; article compares benefits of alkylthiolates on gold SAM systems.

자사의 과학자팀은 생명 과학, 재료 과학, 화학 합성, 크로마토그래피, 분석 및 기타 많은 영역을 포함한 모든 과학 분야에 경험이 있습니다..

고객지원팀으로 연락바랍니다.