모든 사진(2)
About This Item
Linear Formula:
LiBO2
CAS Number:
Molecular Weight:
49.75
EC Number:
MDL number:
UNSPSC 코드:
12352302
PubChem Substance ID:
NACRES:
NA.23
분석:
99.995% trace metals basis
양식:
powder
추천 제품
Quality Level
분석
99.995% trace metals basis
양식
powder
불순물
≤55.0 ppm Trace Metal Analysis
mp
845 °C (lit.)
SMILES string
[Li+].[O-]B=O
InChI
1S/BO2.Li/c2-1-3;/q-1;+1
InChI key
HZRMTWQRDMYLNW-UHFFFAOYSA-N
유사한 제품을 찾으십니까? 방문 제품 비교 안내
신호어
Danger
유해 및 위험 성명서
Hazard Classifications
Acute Tox. 4 Oral - Eye Dam. 1 - Repr. 2
Storage Class Code
13 - Non Combustible Solids
WGK
WGK 1
Flash Point (°F)
Not applicable
Flash Point (°C)
Not applicable
개인 보호 장비
Eyeshields, Gloves, type N95 (US)
N S Prasad et al.
Journal of nanoscience and nanotechnology, 1(4), 425-432 (2003-08-14)
Transparent glass composites in the system (100 - x) Li2B4O7 - x SrBi2Nb2O9 (where x = 5, 10, 15, 20, 25, and 30, in molar ratio) were fabricated by conventional melt-quenching technique. The amorphous nature of the as-quenched glass composites
R Gauderon et al.
Microscopy research and technique, 47(3), 210-214 (1999-11-02)
We investigated the effect of a finite-sized confocal pinhole on the performance of nonlinear optical microscopes based on two-photon excited fluorescence and second-harmonic generation. These techniques were implemented using a modified inverted commercial confocal microscope coupled to a femtosecond Ti:sapphire
J Graetz et al.
Nanotechnology, 20(20), 204007-204007 (2009-05-08)
The local bonding and atomic environments in the Ni-catalyzed destabilized system LiBH4/MgH2 and the quaternary borohydride-amide phase Li3BN2H8, were studied by x-ray absorption spectroscopy. In both cases the Ni catalyst was introduced as NiCl2 and a qualitative comparison of the
R Bojanowski et al.
TheScientificWorldJournal, 2, 1891-1905 (2003-08-16)
A simple and rapid method has been developed to determine 226Ra in rocks, soils, and sediments. Samples are decomposed by fusion with lithium metaborate and the melt is dissolved in a solution containing sulfates and citric acid. During the dissolution
Frank R Wagner et al.
Optics express, 18(26), 26791-26798 (2011-01-05)
Multiple pulse nanosecond laser induced damage in the bulk of LiB3O5 (LBO) crystals was investigated at 1064 nm, 532 nm and 355 nm. Scanning electron microscopy of cleaved damage sites confirmed the presence of different zones that have already been